TECHNET Archives

May 2003

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
"Dobbs, Marie" <[log in to unmask]>
Date:
Fri, 23 May 2003 13:09:17 -0400
MIME-Version:
1.0
X-To:
"Tempea, Ioan" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Dobbs, Marie" <[log in to unmask]>
Parts/Attachments:
text/plain (58 lines)
Volume Volume and Volume usually dictate SMT VS TH.
If you volume is great enough than SMT is the way to go even if you need to
Loose load a couple of components at hand assembly.  I am not sure which
tech bulletin or procedure would point you in this direction, but that is
how business is done here at Tyco.
Regards
Marie

-----Original Message-----
From: Tempea, Ioan [mailto:[log in to unmask]]
Sent: Friday, May 23, 2003 12:34 PM
To: [log in to unmask]
Subject: [TN] Through-hole design vs. SMT design


Hi Technos,

I have a dilemma on my hands. An assembly that has about 15 passives (caps
and resistors), a connector and a fuse holder. The connector must be TH and
probably so does the fuse holder. The designers came with the question: "for
lower manufacturing costs should we design the board 100% TH, or make the
passives SMT and keep the other 2 parts TH". Interesting...

And here come my questions:

*       what are the technical criteria that you use when trying to solve
this kind of riddle?
*       what are the economical criteria?
*       what parameters could I use for a breakeven analysis?

Thank you,
Ioan

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2