Yes, we also build class 3 and spot-bond all thru-hole components prior to
wave solder. Without this, there is too much part movement to assure a good
joint every time. In our case, the effort is worth it, so we continue with
success.
R. G. Blomberg
Honeywell International
Space Systems
Staff Production Engineer
(727) 539-5534 voice
727-539-4469 Fax
[log in to unmask]
-----Original Message-----
From: Kenny Bloomquist [mailto:[log in to unmask]]
Sent: Wednesday, January 05, 2000 10:54 AM
To: [log in to unmask]
Subject: [TN] Component Stabilizing for Wave Solder
Hello Fellow TechNeters,
We build Class 3 hardware per J-STD-001 and stabilize every through hole
component prior to wave solder. I believe this is a hold over from Mil.
Spec. days and wondering if anyone else is doing this. The requirement per
J-STD-001 is to "process in a manner that precludes movement that
detrimentally affects formation of acceptable solder connections."
To stabilize or not to stabilize, that is the question.
Thank you,
Ken Bloomquist
Sr. Principal Process Engineer
PRIMEX Aerospace Company
P.O. Box 97009
Redmond, WA 98073-9709
http://www.primextech.com
Ph: 425-885-5000
FAX: 425-882-5786
[log in to unmask]
Northcon/2000, Chairman of the Board
http://www.northcon.org
Electronics Manufacturers Association (EMA), President
http://www.ema-wa.org
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|