Currently we are experiencing solder bridging on a 0.5mm pitch,  LQFP,  144
leads. I already reviewed the stencil design, screen printer parameters and
reflow profile. Everything is OK. We have HASL boards. Our current process
outputs 38 dpmo's. My concern is if I reduce more the apertures, I have the
risk to have solder open or insufficient solder, instead of bridging. Does
anybody has some input? What dpmo's do you have?

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2