TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
JASON CROSS <[log in to unmask]>
Date:
Mon, 5 Nov 2001 09:24:24 -0500
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (32 lines)
Hello,
I am hoping someone here can help with the following:  recent inquiries
have come up with respect to the effect of BGA rework to surrounding
components.  Can the heat effect to surrounding components -- the
possibility (and probability) that they will reach reflow temperatures,
cause problems?  I am thinking of cases where some BGA balls might reach
reflow temperatures and others might not on a single package at
proximity to the reworked site.  Another case would be where BGA
packages at proximity to the reworked BGA are simply reaching high
temperatures - for possibly many heat/rework cycles..

Impact to solder joint metallurgy
Impact to solder joint reliability

Any help or reference would be greatly appreciated.

--
Jason Cross
Physical Technology Engineer
Alcatel Canada, Inc.
(613) 784-4793

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2