TECHNET Archives

June 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jean-Francois Bissonnette <[log in to unmask]>
Date:
Thu, 2 Jun 2011 13:51:25 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Upton, Shawn" <[log in to unmask]>
Message-ID:
Subject:
From:
"Upton, Shawn" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (50 lines)
How far from the end of the component was the bend?  I can't tell from the pic.  I wonder if chipping is bound to happen if the components must be bent that close to the body.  That is to say, that chipping is inevitable due to the bend being that close; if the PCB design requires it that close, well, it's inevitable to have either lots of thrown-out resistors, or assemblies with resistors that are chipped.

AFAIK that is just paint chipping, not damage to the resistive element.

Shawn Upton, KB1CKT
Test Engineer
Allegro MicroSystems, Inc
[log in to unmask]
603.626.2429/fax: 603.641.5336

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jean-Francois Bissonnette
Sent: Thursday, June 02, 2011 1:31 PM
To: [log in to unmask]
Subject: [TN] How much damage is too much damage?

Hi Technetters,

 

I would like to have your thoughts on these damages on resistors.  The
picture section 9 of IPC (rev D) shows the middle of the resistor where the
cracked occurred.  In our case, the damage is more on either end of the
body.  Is it just as bad or could this be considered acceptable?

 

http://ipc-technet.groupsite.com/galleries/show/20088

 

Jean-François



______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2