Kris,
Although not quantitative, I was impressed with some SEM's (Scanning
Electron Microscope)
pictures taken of some gold plated Duroid boards that were not performing as
expected. The pictures showed globular deposits of gold on the top surface.
Where the globular deposits didn't
touch, nickel was clearly showing.
Ron VandenDolder
Product Development Group
Telaxis Communications
SouthDeerfield, MA
413-665-8551
-----Original Message-----
From: Kris Keating [mailto:[log in to unmask]]
Sent: Thursday, December 13, 2001 2:31 PM
To: [log in to unmask]
Subject: [TN] porosity of gold plating on nickel
Does anyone know of a fairly simple method of determining porosity of gold
plating over nickel on a PCB?
Kristopher J. Keating
Technical Service Engineer
Circuit-Wise, Inc.
400 Sackett Point Rd.
North Haven, CT 06473
Tel. (203) 281-6511
Fax (203) 287-8409
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|