Paul,

I believe the EMPF in Indianapolis has a process for that or was working on
one. You can check them out at http://www.empf.org/html/empfset.htm

Ken Bloomquist

-----Original Message-----
From: Paul Truit [mailto:[log in to unmask]]
Sent: Wednesday, May 15, 2002 10:41 AM
To: [log in to unmask]
Subject: [TN] Restoring solderability


With today's economic climate we have found that a few parts have been
sitting too long in inventory.  The solderability has been affected.
Specifically it was a two pin terminal block that was shipped to us in a
cardboard box and the part was pressed down into styrofoam. I believe
the sulfur from the cardboard box has out gassed and negatively affected
the part's solderability.

Is there a method to effectively and efficiently restore the
solderability?

TIA
--
Paul Truit, Mfg. Eng.
RBB Systems, Inc.
4265C E. Lincolnway
Wooster, OH  44691
Ph. (330) 567-2906 ext 514
Fax (330) 263-5324
Email: [log in to unmask]

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2