TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Joseph Fjelstad <[log in to unmask]>
Date:
Sat, 29 Nov 1997 13:52:00 +0100
Reply-To:
Subject:
From:
Achim Neu <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=iso-8859-1
Organization:
prv
MIME-Version:
1.0
Parts/Attachments:
text/plain (99 lines)
HI Joseph,

can you shear us some information about reliability of such BGA or CSP
compared with standard TSOP packages soldered on board?

It will interessting to get a feling about the advantages of this
technology.

Greetings
Achim

Joseph Fjelstad wrote:

> Hello Bev,
>
> You had a very complete set of options for Sven-Erik but there is
> another
> option that is also making its way in as an alternative, the µBGA®
> CSP. It
> offers a compliant structure that mitigates the stresses resulting
> from the
> CTE mismatch between the silicon and FR-4 that Werner Englemaier has
> been so
> long warning us all about. In addition, it has a coarser lead pitch, a
>
> smaller proilfe and a can be placed using a chip shooter at rates up
> to
> 20,000 uph at near 100% yields. While presently aimed primarily at
> packaging
> flash memory, it is being targeted to replace the existing TSOP
> packages by
> a number of IC manufacturers around the world based on the demands of
> their
> users.
>
> Cheers!
> J. Fjelstad
>
> >Sven-Eric,
> >TSOPs on FR-4 with a high daily temperature swing are not reliable.
> >There are many papers out in the open literature that substantiate
> this.
>  >Recently Jean Paul Clech (hope I spleed that right) had a little
> >article in the SMT newsletter saying as much, also.  I am also sure
> that
> >Werner Englemaier, another reliability expert, would also agree.
> >
> >You have several options
> >1) ignore the problem and hope that your product becomes obsolete or
> >breaks for another reason
> >2) go to Thermount (aramid) or Ceracom (ceramic) boards
> >3) lower the temperature swings of your product (eg don't sell you
> >portable phone in Minneapolis)
> >4) use a different part type (eg SSOP)
> >5) embed the leads in a underfill material (so far not reworkable,
> >although rumors have it that we should see something in this area in
> >1998)
> >6) get TSOPs with the longest, thinnest leads possible
> >7) wait for the new TSOPs with copper lead frames which are going to
> >replace the Alloy-42 currently used in most of them today.
>
> Good luck!
>
> Bev Christian
> Nortel
> Tessera ...System Building Blocks for the Next Generation of
> Electronics
>  3099 Orchard Drive
>  San Jose, CA 95134
>  Phone 408 894-0700
>  Fax   408 894-0768
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
> 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2