TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Hinners Hans CIV WRALC/LYPME <[log in to unmask]>
Date:
Fri, 27 Aug 1999 13:02:42 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Graham Naisbitt <[log in to unmask]>
Parts/Attachments:
text/plain (100 lines)
Hans

Let me be the first to wish you a Happy Anniversary!

As to removing the coating - HumiSeal have some purpose made strippers which
you might want to try. I am sure the others do too!

However, I can also task you to try PEG (polyethyleneglycol) or PPG
(polypropyleneglycol) - takes a little longer but it do work.

Proprietary strippers are safer because they have been developed for the
suppliers own material.

Regards,
Graham Naisbitt

[log in to unmask]

WEB: http://www.concoat.co.uk

CONCOAT Ltd
Alasan House, Albany Park
CAMBERLEY GU15 2PL UK

Tel: +44 (0) 1276 691100  Fax: +44 (0) 1276 691227
----- Original Message -----
From: Hinners Hans CIV WRALC/LYPME <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, August 26, 1999 2:04 PM
Subject: [TN] Acrylic Conformal Remover which doesn't touch Epoxy? - Does it
e xist


> Hey Everybody,
>
> I'm looking for an acrylic conformal coating remover which won't touch
> epoxy.
>
> I tried Kyzen's Conformox AU and it changed the physical appearance of the
> epoxy - dulled it.
> I should run a hardness test but I think it softened it too.
>
> The current plan uses Trans LC and that leaves a hazy residue.
> This residue does come off when I run it through our Aqueous Cleaner or
get
> the q-tips out but . . .
> an extended soak in Trans LC will soften the epoxy too, so I'm highly
> motivated to find an alternative.
>
> I'm not familiar enough with the properties of acrylic and epoxy to know
> whether I'm trying to defy physics (yet!).
> Somebody out there in cyberland must have faced this opportunity already.
>
> Hans
>
> 5 more days and I will have been in the Industry for 1 whole year.
>
> Air Force Material Command
> Our mission: develop, deliver and sustain the best products for the
world's
> best Air Force.
> ~~~~~~~~
> Hans M. Hinners                                 WR-ALC/LYPME Bldg. 640
> Materials Engineer                                      380 Second Street,
> Suite 104
> Manufacturing Eng. Sec.                         Robins AFB GA 31098-1638
> 912-926-1970 (Voice) 468 - 1970 (DSN)   912-926-7974 (Fax)
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2