TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
From [log in to unmask] Fri Apr 11 11:
11:51 1997
Date:
Thu, 10 Apr 1997 06:22:56 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/11839
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"jvelo3.0.Uh8.CpCJp"@ipc>
Subject:
From:
"Mark W. Spitnale" <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wFHtE-000BjeC; Thu, 10 Apr 97 06:19 CDT
Old-Return-Path:
X-Mailer:
Windows Eudora Light Version 1.5.2
Message-Id:
Parts/Attachments:
text/plain (64 lines)
Response:

Try to stay away from the 3 and 4 row connectors.  The leads seem to get
bent in the packaging and handling and they are a reel pain in the  @%$#&%.
Also I suggest to not use a SMT connector that requires "hardware"
(nuts,bolts,washers,etc.) for attachment.  This further complicates the
process.  Samtec seems to make a good connector available in several
configurations, some are machine placeable.

                                Mark Spitnale
                                Hughes Defense Communications



>>     I am looking at using surface mount connectors on our assemblies.  
>>     Could anyone give me some feedback on their experiences?  Also what 
>>     brand and type of connectors you have had the most success with.
>>     
>>     Thanks,
>>     
>>     Shaun
>>
>>***************************************************************************
>>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>>***************************************************************************
>>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>>***************************************************************************
>>* If you are having a problem with the IPC TechNet forum please contact   *
>>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>>***************************************************************************
>>
>>
>>
>----------------------------------
>Jeffery L. Hempton              Phone: (219) 429-7335   Fax: (219) 429-4688
>Boardshop Manufacturing Engineer			Mail Stop: 25-31
>Hughes Defense Communications                           
>1010 Production Road, Fort Wayne, IN 46808-4106
>Email: [log in to unmask]
>
>"Those who dream by day are cognizant of many things which escape those who
>dream only by night"    - -Edgar Allen Poe
>
>
>
----------------------------------
Mark W. Spitnale                Phone: (219) 429-5992   Fax: (219) 429-
Hughes Defense Communications                           Mail Stop: 25-31
1010 Production Road, Fort Wayne, IN 46808-4106
Email: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2