TECHNET Archives

September 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Dave Chapman <[log in to unmask]>
Date:
Thu, 19 Sep 2002 12:32:54 -0500
MIME-Version:
1.0
X-To:
Henry Rekers <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Dave Chapman <[log in to unmask]>
Parts/Attachments:
text/plain (128 lines)
We had the same complaints of "Cold Solder" when we switched to Immersion
Silver boards. It is a matter of education for manufacturing as well as
customers. Alpha Metals (Alpha Level ) silver process as well as Mac Dermid
have good pictures to show as examples. I'm sure the gold suppliers have
also.
Dave C.

-----Original Message-----
From: Henry Rekers [mailto:[log in to unmask]]
Sent: Thursday, September 19, 2002 10:49 AM
To: [log in to unmask]
Subject: Re: [TN] Dull Joint on the Gold plated PCB.


As with our inspectors, you might start to get complaints of "non-wetting"
or "de-wetting".  This happened when we switched to gold.  The appearance is
slightly different than HASL.

Henry.

-----Original Message-----
From: Dave Hillman [mailto:[log in to unmask]]
Sent: Thursday, September 19, 2002 6:45 AM
To: [log in to unmask]
Subject: Re: [TN] Dull Joint on the Gold plated PCB.


Hi Poh! The visual appearance of a solder joint is not necessarily an
indicator of a solder joint's reliability. The old "bright and shiny"
criteria should have become extinct but some old habits apparently have a
life of their own. IPC-STD-001B, paragraph 9.2.4 "Solder Connection" is one
reference you can use to demonstrate to your customer that "bright and
shiny" is not a requirement.  Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]





pohkh <[log in to unmask]>@ipc.org> on 09/19/2002 08:18:36 AM

Please respond to [log in to unmask]

Sent by:    TechNet <[log in to unmask]>


To:    [log in to unmask]
cc:

Subject:    [TN] Dull Joint on the Gold plated PCB.


Hi Technetters,

Is there anyone able to help me on having a smooth
shining solder joint on gold-plated PCB.

As I understand that the board with gold-plated gives
a relatively dull joint.

However, I have issue convincing my customer that
this symptom is normal.

Poh

----------------------------------------------------------------------------
-----

Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2