We had the same complaints of "Cold Solder" when we switched to Immersion Silver boards. It is a matter of education for manufacturing as well as customers. Alpha Metals (Alpha Level ) silver process as well as Mac Dermid have good pictures to show as examples. I'm sure the gold suppliers have also. Dave C. -----Original Message----- From: Henry Rekers [mailto:[log in to unmask]] Sent: Thursday, September 19, 2002 10:49 AM To: [log in to unmask] Subject: Re: [TN] Dull Joint on the Gold plated PCB. As with our inspectors, you might start to get complaints of "non-wetting" or "de-wetting". This happened when we switched to gold. The appearance is slightly different than HASL. Henry. -----Original Message----- From: Dave Hillman [mailto:[log in to unmask]] Sent: Thursday, September 19, 2002 6:45 AM To: [log in to unmask] Subject: Re: [TN] Dull Joint on the Gold plated PCB. Hi Poh! The visual appearance of a solder joint is not necessarily an indicator of a solder joint's reliability. The old "bright and shiny" criteria should have become extinct but some old habits apparently have a life of their own. IPC-STD-001B, paragraph 9.2.4 "Solder Connection" is one reference you can use to demonstrate to your customer that "bright and shiny" is not a requirement. Good Luck. Dave Hillman Rockwell Collins [log in to unmask] pohkh <[log in to unmask]>@ipc.org> on 09/19/2002 08:18:36 AM Please respond to [log in to unmask] Sent by: TechNet <[log in to unmask]> To: [log in to unmask] cc: Subject: [TN] Dull Joint on the Gold plated PCB. Hi Technetters, Is there anyone able to help me on having a smooth shining solder joint on gold-plated PCB. As I understand that the board with gold-plated gives a relatively dull joint. However, I have issue convincing my customer that this symptom is normal. Poh ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- ---------------------------------------------------------------------------- ----- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------- ----- --------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------