Hi Joe,
We use them quite a bit for standing off axial parts, and there's a few
boards that we stand off crystals, oscillators, and can transistors too.
We don't use the effervescent type, never have had a problem washing the
normal ones away. We clean in an Electrovert H-500 inline cleaner using
straight DI water, and we have an Electrovert MCS-1000 that we use Kyzen XJN
in. Both machines clean the spacers just fine, with no ill effects with
either machine.
We do quite a bit of conformal coating (Acrylic and Urethane), and never have
had an issue because of the spacers...
Hope this helps,
-Steve Gregory-
> Anyone had success using wash-away spacers during wave-soldering, then
> removing them by aqueous cleaning? We're looking at them mostly to
> control standoff of transistor cans and vertically-mounted resistors.
>
> Looking at the Bivar catalog, spacers come in two types, normal and
> "effervescent", which dissolve more quickly.
>
> Do they wash away completely? Leave any residue that affects conformal
> coat adhesion? Any problems with the materials reacting with the wash
> chemistry, either saponifier or alcohol based?
>
> Joe Kane
> BAE SYSTEMS Controls
> Johnson City, NY
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|