Ken mentions:
> Reliability/Quality Expert,
> How can I select the thermal stress/shock profile for loaded board if I
want
> to precipitate the fab problem. Boards are functionally passed but belongs
> to suspect date code.
>
> I am looking for a profile in the following format.
Hi Ken,
Before you do any testing, a good, root cause failure analysis is
required before specifying a failure acceleration method.
Once you've conclusively identified the specifc cause of your
module failure, you can tailor a stress test to weed out that
specific problem (or fix the root cause failure reason, better yet!)
Without the root cause failure identified, you may end
up spending a lot of money, and potentially ruining a lot
of good modules doing accelerated life/reliability testing,
with minimal return.
Rgds
John
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
John Brewer
Supervisor, Component Engineering
Raleigh, NC
(919)-266-8870
[log in to unmask]
-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|