TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Mon, 5 Mar 2018 18:04:04 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Message-ID:
Subject:
From:
Dwight Mattix <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Given good quality fab and copper (demonstrated via some means like IST or HAST), I'd strip them and focus on solder joint life. The next level assembly is going to be a bigger wearout issue I'd wager.







-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson

Sent: Monday, March 5, 2018 10:01 AM

To: [log in to unmask]

Subject: Re: [TN] Non Functioning pads



Since I was surprised by the answers, I am willing to do some studying on the issue because I thought we had that one nailed down.

But just for the sake of a starting point, what if we had:



   - a typical 8-layer board with vias that are 5:1 max aspect ratio (13 or

   20mil)

   - 1000 boards a year (low volume, not worried about cost of drill bits)

   - high thermal cycling in automotive environment



Would you leave the internal non-functional pads or remove them if you wanted the boards to last 20 years?

What is the MOST ROBUST choice?

Sorry for the repeat question, I thought this issue was settled!



Jack (aka "the new guy")



p.s. that's a joke, because every time I think I know everything, I get slapped!



On Mon, Mar 5, 2018 at 11:47 AM, Jack Olson <[log in to unmask]> wrote:



> I hear ya, brother. and don't think I am arguing with the value of 

> doing the work, but (here I go anyway) One of the major benefits of 

> having the IPC in our industry is that every new circuit board 

> designer that comes along, who doesn't know whether to put that note 

> on his fabrication drawing or not, can learn from the experience of 

> others here. He doesn't have to repeat expensive tests just to verify 

> what is already understood by the consensus of other members that have 

> already contributed time and effort and resources to study the issue.

> (but I hear ya!)

>

> Jbro

>

> On Mon, Mar 5, 2018 at 10:51 AM, Dwight Mattix 

> <[log in to unmask]>

> wrote:

>

>> Yeah, I blew past the thread to busy to contribute last week.

>>

>> All else being equal retaining non-functional pads tends to increase 

>> time to barrel wearout from circumferential cracking at/near the 

>> midline.  One notion being that the pads make for a local lower resin 

>> content region around the via (less expansive dielectric acting on 

>> the copper column to wear it out).

>>

>> Non-func pads don't seem to have much bearing on the actual post 

>> interconnect reliability.  Multiwire anyone?  (speaking of dinosaurs).

>>

>> But back to the barrel wearout thing...  All things are rarely equal. 

>> So if you actually build it and test it (due diligence? That's crazy 

>> talk. Who has time or money for that anymore?), I'd wager you'll get mixed results.

>>  A lot depends on factors like the fabricator's drilling and hole 

>> prep skill, the aspect ratio, material involved, copper weights of 

>> the included NF-pads etc.

>>

>> Leaving non-func pads in, increases the drilling challenge. That 

>> increases things that disrupt the hole and factor in to it's ultimate 

>> reliability. For example, a rougher hole wall is very likely to be 

>> part of the effect of leaving NF pads in. That introduces stress 

>> risers in the holewall topography that can accelerate copper wearout 

>> and crack propogation.

>>

>> So all of that say the original question, "It depends."   :)

>>

>> Do your due diligence. If it really matters, build it and test it. 

>> Better yet, build it both ways and test it. Even better, build both 

>> ways at more than one fab and test it.  You'll be illuminated and 

>> smarter at the end of the exercise than 99 of 100 veteran pwb tech 

>> people seen walking the floor with tacky polo shirts, broken down 

>> posture and done-lops last week at IPC/APEX.

>>

>> cheers,

>> dw

>>

>> -----Original Message-----

>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson

>> Sent: Monday, March 5, 2018 7:49 AM

>> To: [log in to unmask]

>> Subject: Re: [TN] Non Functioning pads

>>

>> I must be behind-the-times on this one.

>> Werner Englemaier used to talk about this all the time, and from my 

>> memory an analogy might be similar to comparing a simple rivet to a 

>> "rivet with ribs". If your goal is a robust product (which a lot of 

>> Class 3's are) then it seems like you would want the extra support. 

>> (I'm not making a statement, I'm repeating what I was taught). I'm 

>> pretty sure I've heard Gary Ferrari recommend keeping them in at 

>> least a half a dozen times in his seminars. Aren't the most common failures in boards related to vias?

>>

>> Maybe I have more learnin' to do on this one, but I'm surprised that 

>> NO ONE responded in favor of keeping the unconnected internal pads

>>

>> Well, since we are talking about vias, I was also advised to require 

>> 1mil hole wall plating, even though the standard is 0.8 (I think). 

>> But for the same reason, the stronger we can make our vias, the less "most common"

>> failures we will have, right? (At Caterpillar, we want the most 

>> robust product we can get for the money) Am I sounding like an old dinosaur now?

>>

>> but really, is EVERYONE removing unconnected inner layer pads?

>> Is "increasing the longevity of drill bits" the dominant theme now?

>>

>> onward thru the fog,

>> Jack

>>

>>

>> .

>> On Tue, 27 Feb 2018 11:12:22 -0600, Larry <[log in to unmask]> wrote:

>>

>> >Is there any reason I cannot remove non functioning pads on the 

>> >inner

>> layers for an Class 3 PCB?

>> >

>> >Many thanks,

>> >

>> >Larry

>>

>

>