TECHNET Archives

March 2018

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jose A Rios <[log in to unmask]>
Date:
Mon, 5 Mar 2018 19:27:39 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Message-ID:
Subject:
From:
Dwight Mattix <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
It's going to add cost. Maybe even a lot of cost. In volume pennies, nickels and dimes get really interesting.



Esp if it's any radio/electronics type pwb with a lot of gnd via stitching.   An 8 layer in auto volumes is going to want to optimize multivariable:  good enough reliability vs minimized price point. 



More pads = slower drill time. 

More NF pads = lower hit count = higher drill bit usage.  

Drill bits on a PTH only boards in volume are a significant consumables cost factor.



 

-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Jose A Rios

Sent: Monday, March 5, 2018 10:44 AM

To: [log in to unmask]

Subject: Re: [TN] Non Functioning pads



I feel that for a typical 8 layer board with the A/R and diameters you’re describing, theres plenty of industry capability to drill that, w/o having to remove unused lands. So it ‘should' be a moot discussion unless a specific fabricator isn’t capable to drill thru 6 internal layers of a small hole. 



> On Mar 5, 2018, at 1:01 PM, Jack Olson <[log in to unmask]> wrote:

> 

> Since I was surprised by the answers, I am willing to do some studying 

> on the issue because I thought we had that one nailed down.

> But just for the sake of a starting point, what if we had:

> 

>   - a typical 8-layer board with vias that are 5:1 max aspect ratio (13 or

>   20mil)

>   - 1000 boards a year (low volume, not worried about cost of drill bits)

>   - high thermal cycling in automotive environment

> 

> Would you leave the internal non-functional pads or remove them if you 

> wanted the boards to last 20 years?

> What is the MOST ROBUST choice?

> Sorry for the repeat question, I thought this issue was settled!

> 

> Jack (aka "the new guy")

> 

> p.s. that's a joke, because every time I think I know everything, I 

> get slapped!

> 

> On Mon, Mar 5, 2018 at 11:47 AM, Jack Olson <[log in to unmask]> wrote:

> 

>> I hear ya, brother. and don't think I am arguing with the value of 

>> doing the work, but (here I go anyway) One of the major benefits of 

>> having the IPC in our industry is that every new circuit board 

>> designer that comes along, who doesn't know whether to put that note 

>> on his fabrication drawing or not, can learn from the experience of 

>> others here. He doesn't have to repeat expensive tests just to verify 

>> what is already understood by the consensus of other members that 

>> have already contributed time and effort and resources to study the issue.

>> (but I hear ya!)

>> 

>> Jbro

>> 

>> On Mon, Mar 5, 2018 at 10:51 AM, Dwight Mattix 

>> <[log in to unmask]>

>> wrote:

>> 

>>> Yeah, I blew past the thread to busy to contribute last week.

>>> 

>>> All else being equal retaining non-functional pads tends to increase 

>>> time to barrel wearout from circumferential cracking at/near the 

>>> midline.  One notion being that the pads make for a local lower 

>>> resin content region around the via (less expansive dielectric 

>>> acting on the copper column to wear it out).

>>> 

>>> Non-func pads don't seem to have much bearing on the actual post 

>>> interconnect reliability.  Multiwire anyone?  (speaking of dinosaurs).

>>> 

>>> But back to the barrel wearout thing...  All things are rarely 

>>> equal. So if you actually build it and test it (due diligence? 

>>> That's crazy talk. Who has time or money for that anymore?), I'd wager you'll get mixed results.

>>> A lot depends on factors like the fabricator's drilling and hole 

>>> prep skill, the aspect ratio, material involved, copper weights of 

>>> the included NF-pads etc.

>>> 

>>> Leaving non-func pads in, increases the drilling challenge. That 

>>> increases things that disrupt the hole and factor in to it's 

>>> ultimate reliability. For example, a rougher hole wall is very 

>>> likely to be part of the effect of leaving NF pads in. That 

>>> introduces stress risers in the holewall topography that can 

>>> accelerate copper wearout and crack propogation.

>>> 

>>> So all of that say the original question, "It depends."   :)

>>> 

>>> Do your due diligence. If it really matters, build it and test it. 

>>> Better yet, build it both ways and test it. Even better, build both 

>>> ways at more than one fab and test it.  You'll be illuminated and 

>>> smarter at the end of the exercise than 99 of 100 veteran pwb tech 

>>> people seen walking the floor with tacky polo shirts, broken down 

>>> posture and done-lops last week at IPC/APEX.

>>> 

>>> cheers,

>>> dw

>>> 

>>> -----Original Message-----

>>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson

>>> Sent: Monday, March 5, 2018 7:49 AM

>>> To: [log in to unmask]

>>> Subject: Re: [TN] Non Functioning pads

>>> 

>>> I must be behind-the-times on this one.

>>> Werner Englemaier used to talk about this all the time, and from my 

>>> memory an analogy might be similar to comparing a simple rivet to a 

>>> "rivet with ribs". If your goal is a robust product (which a lot of 

>>> Class 3's are) then it seems like you would want the extra support. 

>>> (I'm not making a statement, I'm repeating what I was taught). I'm 

>>> pretty sure I've heard Gary Ferrari recommend keeping them in at 

>>> least a half a dozen times in his seminars. Aren't the most common failures in boards related to vias?

>>> 

>>> Maybe I have more learnin' to do on this one, but I'm surprised that 

>>> NO ONE responded in favor of keeping the unconnected internal pads

>>> 

>>> Well, since we are talking about vias, I was also advised to require 

>>> 1mil hole wall plating, even though the standard is 0.8 (I think). 

>>> But for the same reason, the stronger we can make our vias, the less "most common"

>>> failures we will have, right? (At Caterpillar, we want the most 

>>> robust product we can get for the money) Am I sounding like an old dinosaur now?

>>> 

>>> but really, is EVERYONE removing unconnected inner layer pads?

>>> Is "increasing the longevity of drill bits" the dominant theme now?

>>> 

>>> onward thru the fog,

>>> Jack

>>> 

>>> 

>>> .

>>> On Tue, 27 Feb 2018 11:12:22 -0600, Larry <[log in to unmask]> wrote:

>>> 

>>>> Is there any reason I cannot remove non functioning pads on the 

>>>> inner

>>> layers for an Class 3 PCB?

>>>> 

>>>> Many thanks,

>>>> 

>>>> Larry

>>> 

>> 

>> 




ATOM RSS1 RSS2