Hi Stein -
There are a number of water soluble, acid fluxes that you could use for
your tinning operation for several manufacturers. I have seen the Superior
30 work well in several applications. I am surprised that the ESA
specification (this is one spec I have never seen) allows the use of a acid
flux in place of a RMA, especially for space applications. Whatever acid
flux you do choose I would suggest you run some cleanliness tests to assure
yourself that your tinning process does not leave a residue on the
components that could lead to corrosion. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
[log in to unmask] on 09/17/97 06:50:40 AM
Please respond to [log in to unmask]; Please respond to
[log in to unmask]
To: [log in to unmask]
cc: (bcc: David D Hillman/CedarRapids/Collins/Rockwell)
Subject: [TECHNET] Pretinning - Flux
Technetters,
I have some problems pretinning some components stored for 5 years.
The components shall be used in space equipment and according to
ESA-PSS-01-708 we can use rosin based flux (RMA) for pretinning. If
RMA flux are inadequate, corrosive water-soluble acid flux can be
used.
For our components RMA flux does not do the trick.
1) Does anyone know a good method that can be used?
2) Does anyone know suppliers of corrosive water-soluble acid fluxes?
3) We have heard of a flux type called SUPERIOR 30. Can anyone tell me
about suppliers of this flux?
Thanks,
Stein Davidsen
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|