TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
TechNet Mail Forum<[log in to unmask]>
Subject:
From:
Doug Pauls <[log in to unmask]>
Date:
Thu, 18 Sep 1997 09:20:29 -0400
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (24 lines)
Stein,
An alternative to the hazardous acid fluxes is to use an electrochemical
reduction method to change the oxides on your leads back to the pure metal
form.  A mild flux can then be used to solder.  The reduction method is a
technology called ROSA (Reduced Oxide Soldering Activity) and is being
developed by a consortia team lead by Dave Hillman, Rockwell
([log in to unmask]).  You might consider trying this new method
before going to the active fluxes, which require a very thorough cleaning.

Doug Pauls
CSL

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2