Finish 1.10.1 of MIL-STD-171 is Copper Coating, Electrodeposited per
Mil-C-14550 and has 4 Classes.
Class 1 .0010 thick
Class 2 .0005 thick
Class 3 .0002 thick
Class 4 .0001 thick
----------
> From: Steves <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] MIL-STD-171
> Date: Thursday, March 05, 1998 8:05 AM
>
> Does anyone know what the copper plating specification in
> accordance with finish 1.10.1 of MIL-STD-171 is. I am ordering the
> spec today but I would like to find out the answer before I receive
> the spec. Thank you in advance for any help you can give me.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|