Finish 1.10.1 of MIL-STD-171 is Copper Coating, Electrodeposited per Mil-C-14550 and has 4 Classes. Class 1 .0010 thick Class 2 .0005 thick Class 3 .0002 thick Class 4 .0001 thick ---------- > From: Steves <[log in to unmask]> > To: [log in to unmask] > Subject: [TN] MIL-STD-171 > Date: Thursday, March 05, 1998 8:05 AM > > Does anyone know what the copper plating specification in > accordance with finish 1.10.1 of MIL-STD-171 is. I am ordering the > spec today but I would like to find out the answer before I receive > the spec. Thank you in advance for any help you can give me. > > ################################################################ > TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c > ################################################################ > To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: > To subscribe: SUBSCRIBE TechNet <your full name> > To unsubscribe: SIGNOFF TechNet > ################################################################ > Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. > For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 > ################################################################ ################################################################ TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c ################################################################ To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body: To subscribe: SUBSCRIBE TechNet <your full name> To unsubscribe: SIGNOFF TechNet ################################################################ Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information. For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311 ################################################################