Hi Vladimir!
I believe Motorola was after the same issue I'm talking about. Its not that you are shrinking the solder mask to encroach on the pad, you are growing the pad to encroach under the mask. Obviously, its not quite that simple, but you can't grow the pad without running into the mask.
Wayne
________________________________
From: TechNet on behalf of Igoshev, Vladimir
Sent: Tue 3/18/2008 12:55 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
I might be wrong but I think I heard a story that the idea of SMD pads
came out from Motorola as they had had a problem with pads being ripped
off during BGA repair. So, to hold the pads down they changed the design
from non-SMD to SMD.
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne
Sent: Tuesday, March 18, 2008 12:38 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
Hi Werner!
SM holding a pad down???!
No! The pad is held to the laminate material with CONTACT AREA. Make
the pads as big as you can, then control solder flow with the mask. And
make sure the mask has nice vertical walls and leaves no contamination
on the pad.
Wayne
________________________________
From: TechNet on behalf of Werner Engelmaier /*
Sent: Tue 3/18/2008 12:32 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
Hi Wayne,
SMD geometries are stress risers.
If you have a large thermal expansion mismatch, the weakest lik will let
go
first. That may be the SJ or the pad adhesion to the PCB (pad cratering)
or
BGA. Having a SM hold the pad to the BGA is something of a Band-Aid
approach.
Werner
**************
It's Tax Time! Get tips, forms, and advice on AOL Money &
Finance.
(http://money.aol.com/tax?NCID=aolprf00030000000001)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|