Tom,
First find out from your customer if they want a temp cycle test or a
thermal shock test, the primary difference being the rate of temperature
change.
For a thermal shock test, I would recommend using Mil-STD-202, Method 107 as
a starting point. It has some information on soak times at the extremes,
and the number of cycles to perform.
There is another MIL document that encompassed temperature cycling,
including operation at the high and low extremes, but the number escapes me
right now.
Eric Kalgren
Electrical Engineer
Continental Tool and Microwave Company
603-775-5200 ext. 333
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tom Parkinson
Sent: Wednesday, September 13, 2006 2:38 PM
To: [log in to unmask]
Subject: [TN] Temp Testing
Hello DN & TN people
We have a customer that wants us to thermally stress a completed PC assembly
(all the SMT & THT parts are soldered in).
The question comes up as to the temp range and time.
They are suggesting:
Room temp to +150F to -40F to room temp.
I'm concerned because of the populated parts (one is a lithium battery). Not
to mention I have no idea on the time periods from extreme to room temp.
Following this test, an electrical test would be performed.
Any suggestions / Comments??
Thanks
Tom
Tom Parkinson
Quality System Manager - CIT
WinTronics, Inc.
Phone: 724-981-5770 - extension 235
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|