TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 17 Jan 2005 14:09:19 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (106 lines)
This technology is in routine volume use for power circuits (e.g. automotive
engine management systems) but not using thickfilm inks. By and large the
only way to tell the boards are not conventional SMT FR4 is to look at the
reverse, which is just plain aluminium.  (Then you notice no holes / through
components)

Regards 

Mike 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Friday, January 14, 2005 8:22 AM
To: [log in to unmask]
Subject: Re: [TN] Aluminum substrates... any issues?


Old idea, used by the car industry up and then. They searched for a
possibility to put the circuitry directly on the chassis, but it seemed
impractical, so it wasn't successful. We experimented some 20 years ago with
anodized aluminium and thickfilm, but the firing temperatures for silver and
gold prints were too  high. Apparently, your house found a solution on that
problem.

Another interesting idea,which is focused upon now, is SiC spraying on metal
sheets. Withstands very high firing temperatures. SiC on pure Moly ought to
withstand anything. The IMAPS folk ought to know about that...

Ingemar Hernefjord
Ericsson Microwave Systems

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill
Sent: den 13 januari 2005 20:08
To: [log in to unmask]
Subject: [TN] Aluminum substrates... any issues?


I ran across this supplier of aluminum boards and was interested if any of
you have dealt with this type of thing before? I have seen metal core boards
made with alumina and bonded with the fiberglass/epoxy for heat sinking
needs but this looks like a different process. Possibly less expensive...
???

http://www.irctt.com/pdf_files/thickfilm_aluminum.pdf

Any comments on it are appreciated.

Best regards,

Bill Brooks - KG6VVP
PCB Design Engineer , C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
e-mail:[log in to unmask]
http://www.dtwc.com
http://pcbwizards.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2