TECHNET Archives

April 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Gumpert, Ben" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gumpert, Ben
Date:
Tue, 5 Apr 2016 10:10:12 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (30 lines)
Seet Leng,

I haven't looked at this defect description before, but it appears that splatter and webbing are two terms indicating essentially the same defect, although webbing might be used when the solder splashes are distributed across an area and splatter refers to splashes that are more contained. 

Ben

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ong Seet Leng
Sent: Tuesday, April 05, 2016 1:27 AM
To: [log in to unmask]
Subject: EXTERNAL: [TN] QUERIES

Afternoon Tech netters,

Apologize for asking the same question again. I may not have put it correctly in my email send yesterday. Here it is: how do one tell the difference between a solder splatter and solder webbing especially to someone who has no knowledge of soldering anomalies. At a first glance, it may look the same and cannot differentiate between them.

Please advise.

Regards,
Seet Leng

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2