Seet Leng, I haven't looked at this defect description before, but it appears that splatter and webbing are two terms indicating essentially the same defect, although webbing might be used when the solder splashes are distributed across an area and splatter refers to splashes that are more contained. Ben -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ong Seet Leng Sent: Tuesday, April 05, 2016 1:27 AM To: [log in to unmask] Subject: EXTERNAL: [TN] QUERIES Afternoon Tech netters, Apologize for asking the same question again. I may not have put it correctly in my email send yesterday. Here it is: how do one tell the difference between a solder splatter and solder webbing especially to someone who has no knowledge of soldering anomalies. At a first glance, it may look the same and cannot differentiate between them. Please advise. Regards, Seet Leng ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the Symantec Email Security.cloud service. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________