TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (AZ75)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (AZ75)
Date:
Thu, 2 Dec 2004 10:17:16 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (144 lines)
Hence the saying "that will only happen when pigs fly".
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Blair K. Hogg
Sent: Thursday, December 02, 2004 6:14 AM
To: [log in to unmask]
Subject: Re: [TN] FOD Prevention training


A company I worked at once had a piece of equipment returned from the field,
failed in flight.

During our investigation we found a piece of ham from a sandwich inside the
unit, causing the failure.

About that time we implemented a policy of no eating or drinking at your
workstation.

Blair

>>> [log in to unmask] 12/02/04 06:19AM >>>
I went through FOD questions a couple years ago with Boeing. I asked the guy
if they had ever found anything with our product. The answer was no. No more
questions.

-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, December 01, 2004 5:13 PM
To: [log in to unmask]
Subject: Re: [TN] FOD Prevention training

Yeah Jason...'member the Chiefs barking at us during FOD walkdown;  "Hands
out of your pockets! Eyes down on the deck!!!"

I thought that the Navy was the last time I would hear that. But, we just
got asked about our FOD control procedures during a recent audit by  Bell
Helicopter/Textron. We addressed it here by showing them our emphasis  to
5-S, and
our standing "Take the last 30-minutes of your shift to clean  your area."
That
seemed to satisfy them...but they did say it would be nice if  we had a
"formal" procedure...

-Steve Gregory-

Man, I  haven't heard that term since my USN days.

Jason  Gregory
Manufacturing Engineer
Innova  Electronics
(281)653-5593
(281)653-5594 fax
(281)310-7588  cell
[log in to unmask]


-----Original Message-----
From:  TechNet [mailto:[log in to unmask]]On Behalf Of Marsico, James
Sent:  Wednesday, December 01, 2004 2:46 PM
To: [log in to unmask]
Subject: [TN]  FOD Prevention training


Good day Technet:
I'm looking for a  training video for FOD (foreign object debris, or foreign
object damage)  prevention, specifically for electronics manufacturing.
Any
recommendations?

Jim Marsico
Senior Engineer
Production  Engineering
EDO Electronics Systems Group
[log in to unmask]  <mailto:[log in to unmask]>
631-595-5879




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


*******************************************************************
This email and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom they
are addressed. If you have received this email in error please notify
the system manager.

This footnote also confirms that this email message has been swept
for the presence of computer viruses.

www.hubbell.com - Hubbell Incorporated

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2