Polyurethanes and acrylics are both used a lot. Acrylics have the
performance most people need and can be removed for mod or rework simply
with localized application of a solvent. This is both an advantage and
disadvantage in that it indicates a low resistance to solvents. Urethanes
are tough with good performance , however, once cured, they can only be
removed by burning or abrasion (scraping) for rework. We use both and have
applied them with selective coating equipment and by hand (spray and brush).
Drying can be in ambient air, conveyor oven or bake oven. Solvent systems
are the most forgiving (I think) but have VOCs. Waterborne also can work
well but need a slower drying. Urethane and acrylics are both available in
100% solids, UV cured versions.
George
-----Original Message-----
From: Fred Pescitelli [mailto:[log in to unmask]]
Sent: Friday, June 06, 2003 8:52 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Systems
What is the preferred chemistry for conformal coating? I hear a lot are
using Acrylic, is that Air dried?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stolar, Paul W
Sent: Wednesday, June 04, 2003 5:16 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal Coating Systems
Both are very good systems. I bought a Nordson, just because I was used to
the operating system. Both systems have their advantages.
Paul Stolar
Materials Engineer
Houston Technology Center
Baker Atlas
713-625-5376
713-625-4949 (fax)
-----Original Message-----
From: Noble, Ed [mailto:[log in to unmask]]
Sent: Wednesday, June 04, 2003 3:39 PM
To: [log in to unmask]
Subject: [TN] Conformal Coating Systems
Hello All,
Looking for comments regarding Conformal Coating Systems. I'm aware of
several systems, seen a few, and narrowed it down to Asymtek/Nordson or PVA.
We'll be dispensing HumiSeal Acrylic Materials.
Would appreciate any feedback from the masses.
Thank You and Appreciate Your Time,
Ed Noble
Process Control Supervisor
[log in to unmask]
Industrial Scientific Corp.
www.indsci.com
voice 412.490.1884
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|