TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Graham Collins <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 8 Jul 2008 12:44:30 -0300
Content-Type:
text/plain
Parts/Attachments:
text/plain (87 lines)
Hey guys.
Thanks for all the opinions and info.  I'm stuck in the middle, on one
side is a designer saying that it means pre-finishing size, on the other
I've got a fabricator saying it means finished hole size.  The drawing
is ambiguous on this point.  I just want parts to build things with!!!

I do agree with Werner that it does not matter as they are only vias,
but once someone had inspected and measured something it became a
debate. 


regards,
 - Graham

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Monday, July 07, 2008 7:57 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size

Hi Werner,

I like your thinking but... 

I'm not in the quality department, no offense to those of you who are,
but I wouldn't want to be ;-) But thinking like an inspector, how would
you verify that you got the right size holes if you don't call out a
finished hole size? I guess you could do a cross section but a pin gage
is a lot simpler.

Just thinking out loud,

KennyB

-----Original Message-----
From: Werner Engelmaier /* [mailto:[log in to unmask]]
Sent: Monday, July 07, 2008 3:36 PM
To: [log in to unmask]
Subject: Re: [TN] Flex specifications - tolerance on hole size

Hi Graham,
Why do you care what the finished hole size is? Do you put component
leads into 0.028"/+- 0.003" holes, that is 25 mils minimum?
The finished hole size specifications are an anachronism harking back to
the

THT-days-today they only should be specified for componet lead holes.
For vias the drilled hole diameter should be specified-it is much more
important.
Werner
Future workshops:
Pb-Free Soldering Processes-Survival, Quality, Reliability, July 17/18,
Thal, Switzerland Pb-Free Soldering Processes-Survival, Quality,
Reliability, July 21/22, Bad Segeberg, Germany Pb-Free Soldering
Processes-Survival, Quality, Reliability, August 18, Orlando Reliability
Issues with Lead-Free Soldering Processes, September 22, Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle
Fracture,

ENIG), September 22, Schaumburg
Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia Solder
Joint Reliability: Parts 1 & 4, Oct. 17, Timisoara, Rumania Solder Joint
Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2