Hey guys. Thanks for all the opinions and info. I'm stuck in the middle, on one side is a designer saying that it means pre-finishing size, on the other I've got a fabricator saying it means finished hole size. The drawing is ambiguous on this point. I just want parts to build things with!!! I do agree with Werner that it does not matter as they are only vias, but once someone had inspected and measured something it became a debate. regards, - Graham -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist Sent: Monday, July 07, 2008 7:57 PM To: [log in to unmask] Subject: Re: [TN] Flex specifications - tolerance on hole size Hi Werner, I like your thinking but... I'm not in the quality department, no offense to those of you who are, but I wouldn't want to be ;-) But thinking like an inspector, how would you verify that you got the right size holes if you don't call out a finished hole size? I guess you could do a cross section but a pin gage is a lot simpler. Just thinking out loud, KennyB -----Original Message----- From: Werner Engelmaier /* [mailto:[log in to unmask]] Sent: Monday, July 07, 2008 3:36 PM To: [log in to unmask] Subject: Re: [TN] Flex specifications - tolerance on hole size Hi Graham, Why do you care what the finished hole size is? Do you put component leads into 0.028"/+- 0.003" holes, that is 25 mils minimum? The finished hole size specifications are an anachronism harking back to the THT-days-today they only should be specified for componet lead holes. For vias the drilled hole diameter should be specified-it is much more important. Werner Future workshops: Pb-Free Soldering Processes-Survival, Quality, Reliability, July 17/18, Thal, Switzerland Pb-Free Soldering Processes-Survival, Quality, Reliability, July 21/22, Bad Segeberg, Germany Pb-Free Soldering Processes-Survival, Quality, Reliability, August 18, Orlando Reliability Issues with Lead-Free Soldering Processes, September 22, Schaumburg Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture, ENIG), September 22, Schaumburg Solder Joint Reliability: Parts 1 & 4, Oct. 9, Moscow, Russia Solder Joint Reliability: Parts 1 & 4, Oct. 17, Timisoara, Rumania Solder Joint Reliability: Parts 1 & 4, Oct. 22, Tallinn, Estonia --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------