TECHNET Archives

December 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 7 Dec 2009 09:15:48 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Content-Transfer-Encoding:
quoted-printable
From:
Charming Chan <[log in to unmask]>
Parts/Attachments:
text/plain (23 lines)
Hello All, 

I'm asking for help to understanding the section R6-176 and R7-13 in spec TELCORDIA GR-78-CORE Issue 2, thanks a lot.

R6-176 [336] Insulation thickness between adjacent PTHs and conductors shall be a minimum of 0.004 inch(0.0035 inch after accounting for isolated protrusions).  

Question: Does this section mean that the spacing between PTHs and conductors shall be a minimum of 0.004 inch?


R7-13 [426] Interconnection and circuit pack design rules shall include an interconductor voltage limit where wet(screen printed) solder masks are used. Above this voltage, dry film or demonstrated equivalent photoimageable wet solder mask shall be used; conformal coatings are a viable alternative.

Question: What's the specific voltage limit shall set up for wet solder mask?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2