J-STD-006A, Requirements for Electronic Grade Solder Alloys and Fluxed and Non-Fluxed Solid Solders for Electronic Soldering Applications
This standard prescribes the nomenclature, requirements and test methods for electronic grade solder alloys; for fluxed and non-fluxed bar, ribbon, and powder solders, for electronic soldering applications; and for "special" electronic grade solders. The most prominent change introduced by Revision A is a new alloy nomenclature system. Supersedes QQ-S-571. Released May 2001. 18 pages.
To see a list of the latest releases,
- go to www.ipc.org
- click on "Catalog/Bookstore"
- click on "New Releases"
Member Price: $20 Non-Member Price: $40
To order by:
PHONE: 847.790.5362
FAX: 847.509.9819
EMAIL: [log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|