text/plain (59 lines)
Doug

Citric acid is a funny one. It is tribasic (compared with dibasic for
most of the other usual N/C activators). Hughes are not the only one to
come unstuck with citric: Zeva had a citric acid/glycerol (a triol or
tribasic alcohol) W/S flux in the 1970s, long before Hughes. I believe
that the problem with citric is that it forms unstable chelates with
some heavy metals (don't drink lemonades etc. from lead crystal or
lead-containing pewter vessels!). The later formulations were, I
believe, with maleic acid (found in green apples), which is dibasic. Its
ages since I heard anything about HF fluxes: I thought they had died a
natural death.

I had a really bumper crop of lemons this winter, so my personal citric
to maleic ratio has increased enormously :-)

Brian

Douglas Pauls wrote:
>
> Very interesting, Jim. Do you happen to know who made the HF series of
> fluxes? I would like to get data sheets on them.
>
> The original HF1189 was based on citric acid (lemon juice) as the
> activator.  The HF stood for Hughes Flux.  When it first came out, it was
> hailed as the greatest thing since sliced bread.  A classic case of a
> marketing department gone amuck.  The citric acid can be corrosive and
> there were some memorable military failures as a result.  Several studies
> were done on the 1189.
>
> I believe Kester picked up the 1189 family.  They reformulated the
> activator away from citric acid toward more benign weak organic acids and
> called it HF1189A.  If I recall, the 1189A contains no citric acid.
>
> I suggest you contact Kester for more information.
>
> Doug Pauls
> Rockwell Collins
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2