TECHNET Archives

May 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"McGlaughlin, Jeffrey A" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum." <[log in to unmask]>, "McGlaughlin, Jeffrey A" <[log in to unmask]>
Date:
Fri, 21 May 1999 12:15:18 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (87 lines)
Jack  -

I have used the following for calculating max temp rise allowable:

(Tg-Max Ambient)/safety factor

I.E. Tg = 180 deg C
        Max Ambient = 80 deg C
        Safety Factor = 2.5
       Allowable Temp Rise = 40 deg C

It isn't real scientific and I often fudge the safety factor to get closer
to some nominal value but it gives you some place to start.

Jeffrey A. McGlaughlin
PCB Designer
Battelle Memorial Institute
Columbus Ohio
[log in to unmask]


        -----Original Message-----
        From:   Jack Olson [SMTP:[log in to unmask]]
        Sent:   Friday, 21 May, 1999 12:00
        To:     [log in to unmask]
        Subject:        [TN] Temperature Curves for PCB Traces

        Sorry for posting this here (after already trying the designer
council) but
        if I don't get a logical scientifical semi-provable response I will
be
        forced to use the dreaded "10 degree curve" for the rest of my
designs....
        ouch!


        I can't figure out how to select the appropriate temperature curve
when
        calculating PCB trace widths versus current requirements.
        If you use the chart in IPC-D-275 or IPC-2221, you have to select a
curve to
        get your minimum trace width.
        If you use a calculator, it will solve for the temperature rise, but
you
        still must know if it is acceptable.
        So what is acceptable? Anything that won't make the material hit Tg?
        I'm trying to avoid the dreaded "Just use the worst case"...
        Am I missing something?

        ################################################################
        TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
        ################################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
        To subscribe:   SUBSCRIBE TechNet <your full name>
        To unsubscribe:   SIGNOFF TechNet
        ################################################################
        Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
        For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
        ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2