TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vl2n8-0000erC; Thu, 16 Jan 97 19:08 CST
Content-Type:
text/plain; charset="us-ascii"
From [log in to unmask] Fri Jan 17 09:
29:45 1997
Date:
Thu, 16 Jan 1997 14:33:38 -0800 (PST)
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9332
Posted-Date:
Thu, 16 Jan 1997 14:33:38 -0800 (PST)
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"sZ9_f.0.mZM.54jto"@ipc>
Subject:
From:
Old-Return-Path:
<TechNet-d-request>
Mime-Version:
1.0
X-Mailer:
Windows Eudora Light Version 1.5.4 (16)
Message-Id:
Parts/Attachments:
text/plain (46 lines)
OOPS! of course I meant conductor cuts and deleting surface printed
conductor patterns as shown in Procedure 4.2.8 of IPC-R-700C. Deleting
intercinnections is another whole bag of worms. Thanks for helping clarify
this, Jan.

  Doug Whitnell

>At 02:36 PM 1/16/97Jan Satterfield ( [log in to unmask]) wrote
>
>What are connector cuts and deleting surface connectors???  Is there a 
>possibility that you mean conductor cuts and surface conductors?
> ----------
>From: MTTC
>>Subject: ASSY: Jumpers and cuts
>Date: Thursday, January 16, 1997 9:30AM
>We have been asked what the commercial standards or specifications are for
>the use of jumpers or connector cuts are in the production of PWBAs.  We
>have already looked at ANSI/J-STD-001B(nothing except for terminal
>connections), IPC-A-610B (Jumpers), ANSI/IPC-R-700C(Jumpers and Deleting
>Surface Connectors).  Any other suggestions or words of advice in these days
>of "acquisition reform"?  What is acceptable these days where we find
>procurement of "off-the-shelf" PWBAs with customizing (jumpers, cuts, racing
>stripes, etc.) so they will perform tthe job.  By the way, Class 3
>electronics.

>
We can be reached at:            e-mail: [log in to unmask]
Manufacturing Technology Training Center (MTTC), Inc
543 Graaf Street                     Phone 619 446-5571 
Ridgecrest CA 93555              Fax  619 446-4337
Web Site: http://www1.ridgecrest.ca.us/~mttc/mttc.htm 
We sponsor The 21st Annual Electronics Manufacturing Seminar
 to be held 19-21 Feb 1997. Contact us for further information.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2