TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
X400-Content-Type:
P2-1988 ( 22 )
Old-Return-Path:
Date:
25 Mar 1997 17:25:53 -0600
From [log in to unmask] Wed Mar 26 08:
32:43 1997
Precedence:
list
Resent-From:
Conversion:
Allowed
Disclose-Recipients:
Prohibited
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
Priority:
normal
X-Loop:
Content-Return:
Allowed
X400-MTS-Identifier:
[/c=US/admd=MCI/prmd=Honeywell/; 0741F33385F01393-HW-MTA-AZ]
TO:
"[log in to unmask]" <[log in to unmask]> (Return requested), "[log in to unmask]" <[log in to unmask]> (Return requested)
X-Mailing-List:
<[log in to unmask]> archive/latest/11476
Return-Path:
<TechNet-request>
Message-Id:
<0741F33385F01393*/c=US/admd=MCI/prmd=Honeywell/o=AZ-MTA/ou=MSMail/ou=CAS/s=Vertefeuille/g=Russ/@MHS>
X400-Recipients:
non-disclosure;
X400-Originator:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w9fSb-000BjCC; Tue, 25 Mar 97 17:16 CST
Resent-Message-ID:
<"RLyoZ2.0.6DH.ep5Ep"@ipc>
Subject:
From:
"Vertefeuille, Russ (AZ77)" <[log in to unmask]>
Alternate-Recipient:
Allowed
X400-Received:
by mta HW-MTA-AZ in /c=US/admd=MCI/prmd=Honeywell/; converted ( IA5-Text); Relayed; 25 Mar 1997 17:25:53 -0600 by /c=US/admd=MCI/prmd=Honeywell/; converted ( IA5-Text); Relayed; 25 Mar 1997 17:25:53 -0600
Original-Encoded-Information-Types:
IA5-Text
Content-Identifier:
0741F33385F01393
Parts/Attachments:
text/plain (60 lines)
My Co. is still using a Hollis Polyclean SMT Plus Aqueous Cleaner.   As far 
as Aqueous cleaners go, it's not one of the largest available on the market 
today. We have been using this cleaner since 1989 with only a few problems. 
 We use a 5% saponifier solution Alpha 2110A.  Cleanliness levels 
consistantly fall below 2 ug/sq. in. as measured with an ionograph 600SMD. 
 Since Hollis Engineering has been taken over by  Alpha/Cookson/Electrovert, 
you must be considering used equipment?????  If you wish to contact me 
offline you may do so @ 602-436-8738
Regards,

Russ Vertefeuille
Sr Proj. Eng.
 ----------
>From: [log in to unmask]
>To: [log in to unmask]
>Subject: GEN-Hollis Cleaners
>Date: Tuesday, March 25, 1997 10:04AM
>
>Date     25/3/97
>Subject  GEN-Hollis Cleaners
>From     Maurice Dore
>To  Tech Net
>
>                      GEN:Hollis Cleaners
>
>Has anyone any info. on Hollis Aqueous Cleaning Systems
>Any users comments etc
>We are thinking of getting a Polyclean , but it looks like a very big
>machine.
>
>All comments appreciated
>
>Thanks in advance.
>
>Moss
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>***************************************************************************
>
>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2