My Co. is still using a Hollis Polyclean SMT Plus Aqueous Cleaner. As far as Aqueous cleaners go, it's not one of the largest available on the market today. We have been using this cleaner since 1989 with only a few problems. We use a 5% saponifier solution Alpha 2110A. Cleanliness levels consistantly fall below 2 ug/sq. in. as measured with an ionograph 600SMD. Since Hollis Engineering has been taken over by Alpha/Cookson/Electrovert, you must be considering used equipment????? If you wish to contact me offline you may do so @ 602-436-8738 Regards, Russ Vertefeuille Sr Proj. Eng. ---------- >From: [log in to unmask] >To: [log in to unmask] >Subject: GEN-Hollis Cleaners >Date: Tuesday, March 25, 1997 10:04AM > >Date 25/3/97 >Subject GEN-Hollis Cleaners >From Maurice Dore >To Tech Net > > GEN:Hollis Cleaners > >Has anyone any info. on Hollis Aqueous Cleaning Systems >Any users comments etc >We are thinking of getting a Polyclean , but it looks like a very big >machine. > >All comments appreciated > >Thanks in advance. > >Moss > >*************************************************************************** >* TechNet mail list is provided as a service by IPC using SmartList v3.05 * >*************************************************************************** >* To subscribe/unsubscribe send a message <to: [log in to unmask]> * >* with <subject: subscribe/unsubscribe> and no text in the body. * >*************************************************************************** >* If you are having a problem with the IPC TechNet forum please contact * >* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * >*************************************************************************** > > *************************************************************************** * TechNet mail list is provided as a service by IPC using SmartList v3.05 * *************************************************************************** * To subscribe/unsubscribe send a message <to: [log in to unmask]> * * with <subject: subscribe/unsubscribe> and no text in the body. * *************************************************************************** * If you are having a problem with the IPC TechNet forum please contact * * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] * ***************************************************************************