Tim,
In addition to the items mentioned by Mike, I'd stress that the preheat is
critical, at least in our expreience. We've found that in general, we've had
to increase preheat times over 'normal' oven profiles. Also, the warping
down at the corners sounds like too much top heat.
Rick Thompson
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of Stammely, Tim
> Sent: Saturday, October 31, 1998 4:29 AM
> To: [log in to unmask]
> Subject: [TN] BGA rework question
>
>
> Hello all,
>
> We are trying to remove and replace two ORCA 432 pin BGA's on
> a big 14-layer
> board. We are getting alot of shorts after the rework(I'm
> x-ray inspecting).
> At first we tried solder pasting the pads with a mini stencil, but the
> amount of bridging we got caused me to try just fluxing the
> pads and letting
> the solder balls collapse, but we still got a lot of shorts. I am also
> noticing a lot of board warpage during the rework heat cycle
> and it also
> appears that during reflow if I watch the component, the
> corners of the BGA
> collapse very early and the component almost appears to be
> bowing. Most of
> the shorts we are getting are in the corners where this last
> observation
> occurs making me think it is causing the shorts. Any
> suggestions on how to
> eliminate this problem?
>
> Thanks,
>
> Tim Stammely
> Manufacturing/Process Engineer
> MSI
> Manassas, VA
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using
> LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask]
> with following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at
> [log in to unmask] or 847-509-9700 ext.312
> ################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|