I count 6 but I can see the dividing lines.
Jack lets see a stack up diagram for this thing please.
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor G. Hernandez
Sent: Wednesday, November 21, 2007 9:15 AM
To: [log in to unmask]
Subject: Re: [TN] Core Quality Issue?
In your statement you counted 10 layers while I only count 6.
I always look at high magnification of each copper foil involved.
A typical core will have 2 foils with the teeth facing each other.
Instance failure or delay.
You state EOL testing, bare board or component testing, functional.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Wednesday, November 21, 2007 10:58 AM
To: [log in to unmask]
Subject: [TN] Core Quality Issue?
Sorry to re-start a previous discussion, but I'm still dealing with a
board failure and I'm trying to learn fast.
I received a higher-resolution picture of a board problem we are having
http://www.frontdoor.biz/PCBportal/corequestion.jpg
<http://www.frontdoor.biz/PCBportal/corequestion.jpg>
Http://www.frontdoor.biz/PCBportal/corequestion.jpg
http://www.frontdoor.biz/PCBportal/corequestion.jpg
and if I look at it closely, I can see the dividing line between all ten
layers of dielectric.
By looking at which way the copper is located from each dividing line, I
can tell which are cores and which are prepreg (because the prepreg
layers will flow "around" the copper features) For example, the thin
pinkish layer is a core. Am I on the right track so far?
So, our problem is a 120V end-of-line test frying two out of every
hundred boards right through the pinkish core material with the white
streak through it
(3.2 mils, which should handle a few kilovolts at least, right?)
So here's the question:
Should I be questioning the material quality rather than the bare-board
manufacturing process itself?
I realize you guys have already been generous with helping me on this,
so I hope I'm not pushing your patience...
onward thru the fog,
Jack (aka "the new guy")
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|