TECHNET Archives

November 2007

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 21 Nov 2007 12:26:47 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Creswick, Steven" <[log in to unmask]>
Subject:
From:
"Creswick, Steven" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (162 lines)
Lastly, 

Back in the olden days, there were more likely to be 'extra' low
molecular weight components [eg - less 'refined' / 'purified'] than in
today's engineering materials - it is my opinion that these played a big
role in generating the 'bad press'.  

Some materials would even revert back to their slimy origins, on
occasion, although not frequently [thankfully] for most of us.  

Am not sure if any of this applies to any silicones in lens cleaner or
not, however.

From here, you can make the intelligent decision as it applies to your
application  :-)

Steve



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter Swanson
Sent: Wednesday, November 21, 2007 9:27 AM
To: [log in to unmask]
Subject: Re: [TN] Silicone Lens Cleaner Problem

Inge,

I would say "right", but only if you replace all the "silicon" with
"silicone"! That last "e" makes a bit difference.

Regards,
Peter

--------------------------------------------------------
Peter Swanson           [log in to unmask]
INTERTRONICS                http://www.intertronics.co.uk
Tel: +44 1865 842842                   Oxfordshire, England

INTERTRONICS is dedicated to providing quality material, consumable 
and equipment solutions to the high technology, high performance 
assembly industries, incorporating outstanding levels of technical 
support and customer service.

Read our news! http://www.intertronics.co.uk/blog/blog.htm

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: 21 November 2007 14:20
To: [log in to unmask]
Subject: Re: [TN] Silicone Lens Cleaner Problem

Most scaring reports about silicon 'oil'smear (spreading, migration ..)
are from the 60's when silicon was found to contaminate relay contacts
and connectors in general. Few incidents were found, but they were
enough to start hysteria. So, silicon was banned and forbidden for (too)
many applications. Still, many are deadly afraid of 'silicon'. People
with a more balanced insight know that there is a variety of silicon
products, most of which can be used without fear. In fact, we use a lot
of silicon glues, silicon O-rings, silicon insulators etc. Then what was
so catastrophic about silicon? I'm not like Brian, a chemistry
specialist, so I may need some correction. I found that:

1. Silicon 'oil' use to be an oil with a very small additive of a
silicon compound.
2. The oil is often a mineral oil, and there are many...
3. The additive is often a polymerized siloxane like dimethylsiloxane or
diphenylsiloxane. 
4. It's the surface energy and the viscosity of the mineral oil, that
decides if the 'silicon oil' will spread or not. If the mineral oil is
'slow', there is little risk of spreading, while a 'rapid' oil may cause
wetting and spreading (or 'migration', if you prefer to use that word).
There are oils with viscosity 200,000 mPa.s and those with viscosity as
low as 40 mPa.s. The time to equilibrium of wetting can vary from days
to seconds.
5. The micro-geometry or topography/porosity of the surface is also an
important factor. If the surface is microscopically very porous, it will
take longer time for the 'silicon oil' to creep into all voids an
supersede air with oil. If the proportion between the viscosity and the
topo/porosity is adverse for the oil, any wetting may be stopped, and
the oil can't creep.
6. So, as so oftenly else, ID(tm)(it depends). You can't ban all silicon
products based on the fear of silicon migration.

Right?

Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: den 12 november 2007 17:14
To: [log in to unmask]
Subject: [TN] Silicone Lens Cleaner Problem


I'm hoping that somenone on TechNet this morning can help my understand
a little more about this. I received a letter from a customer stating
that silicone can introduce contaminants which are detrimental to the
manufacturing process.  The notice specifically mentioned lens cleaner. 

Can someone enlighten me as to what problems silicone can cause?

Thanks,

Blair

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited.  If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.  




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2