Blair,
I can not say that lens cleaners contain silicone, but if you do happen
to have silicone fluids, etc, around they do tend to spread if one is
not reasonably careful.
Have worked with silicone gels for automotive applications [called it
elephant snot] in the same facility as very high rel microelectronics
without incurring problems, but ... but ... but ... proper housekeeping
and handling to prevent cross-contamination is/was very important for
all the reasons other people have mentioned.
Have to read the MSDS for one of the lens cleaners and see if there is
some free silicone in there.
Regarding breast implants - Dow took a really big hit for that. Not
sure of the ultimate epidemiological outcome, but saline does sound a
bit more logical - however the pouch is still a silicone elastomer.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: Monday, November 12, 2007 11:14 AM
To: [log in to unmask]
Subject: [TN] Silicone Lens Cleaner Problem
I'm hoping that somenone on TechNet this morning can help my
understand a little more about this. I received a letter from a customer
stating that silicone can introduce contaminants which are detrimental
to the manufacturing process. The notice specifically mentioned lens
cleaner.
Can someone enlighten me as to what problems silicone can cause?
Thanks,
Blair
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|