Surface analysis techniques such as Auger would shed some light on this.
Bruce Stacy
"Carano,Michael" <[log in to unmask]> on 02/18/99
12:59:09 PM
Please respond to "\"TechNet E-Mail Forum.\" <[log in to unmask]>,
\"Carano,Michael\"" <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Bruce Stacy/ECSDOMAIN)
Subject: Re: [TN] Galvanic reactions
This is a good question. In the past, I have processed boards with both
gold
and tin-lead deposits on the same boards through an alkaline etchant and a
hydrogen peroxide sulfuric acid based etch. We never detected any staining
or darkening of the gold. However, the extent of undercut on the
copper/nickel/gold plated traces was significantly greater than on the
tin-lead/copper traces.
We can attribute that to the galvanic reaction, but do not know if that is
the reason for gold staining.
Best regards,
Mike Carano
> -----Original Message-----
> From: doug smith [SMTP:[log in to unmask]]
> Sent: Thursday, February 18, 1999 11:49 AM
> To: [log in to unmask]
> Subject: [TN] Galvanic reactions
>
> In PCB fabrication process SnPb is used as an etch resist. On some boards
> gold is selectively plated, for example on a BGA pattern. In this case
> both the SnPb and the Au are being used as the etch resist.
>
> The etch process removes unwanted copper leaving the plated circuits and
> component lands.
>
> Can copper staining on gold be the result of a galvanic cell that is
> formed when the nickel/gold and tin/lead are used as an etch resist?
>
> Doug Smith
> Technical Support Engineer
> Yamamoto Mfg. (USA), Inc.
>
> (408)944-8308
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|