TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Wed, 29 Jul 2009 12:47:43 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
Werner,

Just by your answer to Inge, it proves you are still a sound and practical guy. Probably always will be, provided you don't get overheated on the golf course while the rest of us work to keep our jobs.



I had to do a lot of work on this issue while working for Honeywell, and I found out (painfully) that the weight percentage approach alone does not prove/disprove a gold embrittlement issue will or will not occur. It can happen with as little as 1% gold by volume. 

There are many other factors involved, including the shape of the SJs.



And all, once again, remember this is a time-variable phenomena. Nucleation of gold through the SJ takes time. Soldering of gold-plated leads to a circuit board and then performing immediate pull-testing means nothing.



This is the reason that paragraph 3.9.3 of J-STD-001D states what it does. And if you need to build Space product (per J-STD-001DS), the rules are even more stringent; you cannot solder any part containing any amount of gold on the solderable portion of the leads, it must be removed. The only exception is if you can prove with "documented objective evidence available for review that there are no gold-related solder embrittlement problems associated with the soldering process being used."

Good luck with that.



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*

Sent: Wednesday, July 29, 2009 11:54 AM

To: [log in to unmask]

Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT





 Hi Inge,

No 'used to be-—I think I still am.

If you read my resposes you find that I do not think much of this wt-% approach—and it has nothing to do with the impracticality of it after the fact.

Werner





 





 



-----Original Message-----

From: Inge <[log in to unmask]>

To: TechNet E-Mail Forum <[log in to unmask]>; [log in to unmask]

Sent: Wed, Jul 29, 2009 12:41 pm

Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT



















Werner, 

 



You use to be a sound and practical guy. How on earth can you decide the 

volume %-age of the Au brittle phase content in solder joints. Only way is 

chemical analysis of some kind, but how do you know then the weight % of 

respective AuSn phase? 



/Inge 

 





----- Original Message ----- 

From: "Werner Engelmaier /*" <[log in to unmask]> 



To: <[log in to unmask]> 



Sent: Wednesday, July 29, 2009 3:07 PM 



Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT 

 



 



Hi Inge, 



How on earth did you find this gem? 



Not only does it say all that needs to be said to avoid Au-embrittlement, 

but it also points out the misgivings about 



ENIG which certainly have been experienced by many. 



Too bad, we have not heard from the 'Moon Man' in years—thank god we still 

get 'tuppence' from Brian. 



Werner 

 



 



 



 



 





-----Original Message----- 



From: Inge <mm24727@mu

lle.swipnet.se> 



To: TechNet E-Mail Forum <[log in to unmask]>; [log in to unmask] 



Sent: Wed, Jul 29, 2009 3:39 am 



Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT 

 



 



 



 



 



Interesting discussion between Brian Ellis and Earl Moon 11 years ago: 

 



/Inge 

 





http://dev.smtnet.com/Forums/index.cfm?fuseaction=view_thread&CFApp=1&Thread_ID=2345&#Message9513 

 



 



 



 



 



 



 





----- Original Message ----- 

From: "Werner Engelmaier /*" <[log in to unmask]> 

 



To: <[log in to unmask]> 

 



Sent: Wednesday, July 29, 2009 1:20 AM 

 



Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT 

 



 



Hi Thomas, 

 



The attached will have to do. 

 





Werner 

 



Future webinars: 

 



September 15, “Fundamentals in Solder Joint Reliability” 

 



September 16, “Root Cause Analysis of Solder Joint Failures” 

 



September 17, “Solder Joint Reliability for Pb-Free Solders” 

 



Future workshops: 

 



September 24, IPC Midwest, Schaumburg, IL “Fundamentals in Solder Joint 



Re 



liability” 

 



 



 



 



 



-----Original Message-----  



From: Gervascio, Thomas L <[log in to unmask]> 

 



To: [log in to unmask] 

 



Sent: Tue, Jul 28, 2009 6:42 pm 

 



Subject: Re: [TN] FORMULA FOR=2

0DETERMINING GOLD PERCENTAGE IN A SOLDER JOINT 

 



 



 



 



 



 



How could I get a copy of it? I thought EP&P was out of print.. 

 





-----Original Message-----  



From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman 

 



Sent: Tuesday, July 28, 2009 10:01 AM 

 



To: [log in to unmask] 

 



Subject: Re: [TN] FORMULA FOR DETERMINING GOLD PERCENTAGE IN A SOLDER 

 



JOINT 

 





Hi Jon - the folks from Lockheed published a very good article on the 

 



impact of gold on solder joints including the calculations/material 

 



parameters/graphs that would be useful to you. Pull a copy of this 

 



article: "Effects of Gold Diffusion on a Near Eutectic Solder Joint", S. 

 





Enwright, Electronic Packaging & Production, June 1998, pp 68-72. Good 

 



Luck. 

 





Dave Hillman 

 



Rockwell Collins 

 



[log in to unmask] 

 



 



 



"Roberts, Jon (SA-1)" <[log in to unmask]> 

 



Sent by: TechNet <[log in to unmask]> 

 



07/28/2009 07:53 AM 

 



Please respond to 

 



TechNet E-Mail Forum <[log in to unmask]>; Please respond to 

 



"Roberts, Jon ( 

 



SA-1)" <[log in to unmask]> 

 



 



To 

 



[log in to unmask] 

 



cc 

 





Subject 

 



[TN] FORMULA FOR DETERMININ 



G GOLD PERCENTAGE IN A SOLDER JOINT 

 



 



 





 



Does anyone have or know where to find the formula for determining the 

 



amount of percentage of gold in a SMT solder joint?  Appreciate any 

 



help, Jon 

 



 



This communication is intended only for use by the addressee(s) named 

 



herein and may contain business confidential and/or legally privileged 

 



information. If you are not the intended recipient of this e-mail, you 

 



are 

 



hereby notified that any dissemination, distribution, disclosure or 

 



copying of this e-mail and its contents is strictly prohibited. If you 

 



have received this e-mail in error, kindly notify the sender by replying 

 





to this message. In addition, please permanently delete the message and 

 



any attachments without copying or disclosing the contents. Thank you 

 



for 

 



your cooperation. 

 



THIS DOCUMENT AND/OR SHIPMENT MAY CONTAIN COMMODITY ITEMS, SOFTWARE OR 

 



TECHNICAL DATA THAT IS CONTROLLED BY U.S. EXPORT LAW, AND MAY NOT BE 

 



EXPORTED OUTSIDE THE UNITED STATES OR TO NON U.S. PERSONS WITHOUT THE 

 



APPROPRIATE EXPORT LICENSE FROM EITHER THE U.S. DEPARTMENT OF STATE OR 

 



DEPARTMENT OF COMMERCE. 

 





---------------------------------------------------  



Technet Mail List provided as a service by IPC using LISTSERV 15.0 

 



To unsubscribe, send a message to [log in to unmask] with following text 

 



in 

=C

2



the BODY (NOT the subject field): SIGNOFF Technet 

 



To temporarily ha 



lt or (re-start) delivery of Technet send e-mail to 

 



[log in to unmask]: SET Technet=2 

 



0NOMAIL or (MAIL) 

 



To receive ONE mailing per day of all the posts: send e-mail to 

 



[log in to unmask]: SET Technet Digest 

 



Search the archives of previous posts at: 

 



http://listserv.ipc.org/archives 

 



Please visit IPC web site 

 



http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

 



for additional information, or contact Keach Sasamori at [log in to unmask] 

 



or 

 



847-615-7100 ext.2815 

 



-----------------------------------------------------  



 



---------------------------------------------------  



Technet Mail List provided as a service by IPC using LISTSERV 15.0 

 



To unsubscribe, send a message to [log in to unmask] with following text 

 



in 

 



the BODY (NOT the subject field): SIGNOFF Technet 

 



To temporarily halt or (re-start) delivery of Technet send e-mail to 

 



[log in to unmask]: SET Technet NOMAIL or (MAIL) 

 



To receive ONE mailing per day of all the posts: send e-mail to 

 



[log in to unmask]: SET Technet Digest 

 



Search the archives of previous posts at: 

 



http://listserv.ipc.org/archives 

 



Please visit IPC web site 

 



http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 

 



information, or contact Keach

 Sasamori at [log in to unmask] or 847-615-7100 

 



ext.2815 

 



-----------------------------------------------------  





---------------------------------------------------  



Technet Mail List provided as a service by IPC using LISTSERV 15.0 

 



To unsubscribe, send 



a message to [log in to unmask] with following text in 

 



the BODY (NOT the subject field): SIGNOFF Technet 

 



To temporarily halt or (re-start) delivery of Technet send e-mail to 

 



[log in to unmask]: SET Technet NOMAIL or (MAIL) 

 



To receive ONE mailing per day of all the posts: send e-mail to 

 



Listserv@ip 

 



c.org: SET Technet Digest 

 



Search the archives of previous posts at: http://listserv.ipc.org/archives 

 



Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 



for 

 



additional information, or contact Keach Sasamori at [log in to unmask] or 

 



847-615-7100 ext.2815 

 



-----------------------------------------------------  



 



 



 



---------------------------------------------------  



Technet Mail List provided as a service by IPC using LISTSERV 15.0 

 



To unsubscribe, send a message to [log in to unmask] with following text in 

 



the BODY (NOT the subject field): SIGNOFF Technet 

 



To temporarily halt or (re-start) delivery of Technet send e-mail to 



[log in to unmask]: SET Technet NOMAIL or (MAIL) 

 



To receive ONE mailing per day of all the posts: send e

-mail to 



[log in to unmask]: SET Technet Digest 

 



Search the archives of previous posts at: http://listserv.ipc.org/archives 

 



Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 



for additional information, or contact Keach Sasamori at [log in to unmask] or 



847-615-7100 ext.2815 

 



-----------------------------------------------------  



 



 





--------------------------------------------------- 



Technet Mail List provided as a service by IPC using LISTSERV 15.0 



To unsubscribe, send a message to [log in to unmask] with following text in 



the BODY (NOT the subject field): SIGNOFF Technet 



To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL) 



To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest 



Search the archives of previous posts at: http://listserv.ipc.org/archives 



Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815 



-----------------------------------------------------  







 





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2