TECHNET Archives

November 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Syed Ahmad <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Syed Ahmad <[log in to unmask]>
Date:
Thu, 6 Nov 2008 15:40:31 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (100 lines)
Purple plague at the Au/Al interface would be aided by moisture and
contaminants like halides, Sb, etc., sometimes part of the molding compound
as flame retardants.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Thursday, November 06, 2008 7:44 AM
To: [log in to unmask]
Subject: [TN] FW: [TN] AL CU DENDRTIES INSIDE PLASTIC IC

 

 


Subject: Re: [TN] AL CU DENDRTIES INSIDE PLASTIC IC

 

Purple plague is an intermetallic alloy that is formed at the junction

of the Aluminum pad where the Gold bondwire is bonded.  But this is not

a dendrite, it is a "Barny"cle.

Dewey

 

 

  It is a multi-crystalline growth that appears as a dark or

purple ring around the ball of the gold bondwire.  Typically dendrites,

which will grow within a contaminated plastic IC, do not contain gold.

All it takes is the aluminum, moisture, and an electric field.

 

In the past purple plague has been generally caused by high temperature

whether or not the IC is powered.  It usually causes an open circuit

(eventually) due to Kirkendahl voiding at the interface.  With today's

very closely pitched bonding pads the purple plague growth may be able

to bridge between two adjacent bonding pads. 

 

But again, this is not a dendrite.  Dendrites need an electric field to

induce growth, purple plague occurs in the absence of an electric field.

It occurs at some rate continuously, but at normal operating

temperatures grows so slowly that it is not considered a primary factor

in calculating the lifetime of an IC. 

 

mark

 

Mark Woolley

PTRL Laboratory

Avaya,  1300 West 120th Ave,   Area 33,  Westminster, CO, 8023


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2