TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 4 Dec 2006 12:13:09 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Robert Lazzara <[log in to unmask]>
Parts/Attachments:
text/plain (63 lines)
Brian,

Looks funny to me, too, but not due to it being a few holes.

First observation: There's apparent solder mask lifting/blistering. I  expect
to see uniform solder mask even when the substrate exhibits  delamination,
but these views show an effect appearing more like solder mask  blistering than
ply separation.

Second observation: I see solder mask separating from a trace.

Initial thoughts: This is a failure of the solder mask. The mask wasn't
uniformly cured (or there was inadequate surface preparation prior to masking --
or both).

Q1: Is there an available edge-view of the PCB? The closer/the  better.

Q2: Has anyone performed IPC solder mask testing for peel strength  or
solvent resistivity?

Q3: Has anyone cracked open a box that hasn't gone into the field to se if
the condition is pre-existing?


ROBERT LAZZARA
VP, Business Development
T: (800) 560-9457
F:  (800) 878-5566



____________________________________

In a message dated 12/4/2006 11:30:34 A.M. Eastern Standard Time,
[log in to unmask] writes:


The  following files show the two sides of a PCB in a professional
weather  station. This shows four dark areas which the manufacturer has
ascribed to  water penetration. These are centred on a hole. The whole
thing seems funny  to me, as it has happened on only a few of the holes.
I understand that it  was housed in a water-tight case, not very far from
the Pacific coast. I  was not able to ascertain the laminate type, but it
would not surpise me if  it were paper based (FR3?).

Has anyone seen anything like  this?



____________________________________



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2