I'm thinking most of the above -- looks like creep from the plated holes
along the copper excited by the salt-air and the high current density.
Looks like FR-4 glass/epoxy to me. I saw one instance where this had
jumped from the plane area to an adjacent conductor -- may be a fly in
the ointment...Ian
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Lazzara
Sent: Monday, December 04, 2006 12:13 PM
To: [log in to unmask]
Subject: Re: [TN] water water everywhere!
Brian,
Looks funny to me, too, but not due to it being a few holes.
First observation: There's apparent solder mask lifting/blistering. I
expect
to see uniform solder mask even when the substrate exhibits
delamination,
but these views show an effect appearing more like solder mask
blistering than
ply separation.
Second observation: I see solder mask separating from a trace.
Initial thoughts: This is a failure of the solder mask. The mask wasn't
uniformly cured (or there was inadequate surface preparation prior to
masking --
or both).
Q1: Is there an available edge-view of the PCB? The closer/the better.
Q2: Has anyone performed IPC solder mask testing for peel strength or
solvent resistivity?
Q3: Has anyone cracked open a box that hasn't gone into the field to se
if
the condition is pre-existing?
ROBERT LAZZARA
VP, Business Development
T: (800) 560-9457
F: (800) 878-5566
____________________________________
In a message dated 12/4/2006 11:30:34 A.M. Eastern Standard Time,
[log in to unmask] writes:
The following files show the two sides of a PCB in a professional
weather station. This shows four dark areas which the manufacturer has
ascribed to water penetration. These are centred on a hole. The whole
thing seems funny to me, as it has happened on only a few of the holes.
I understand that it was housed in a water-tight case, not very far
from
the Pacific coast. I was not able to ascertain the laminate type, but
it
would not surpise me if it were paper based (FR3?).
Has anyone seen anything like this?
____________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|