I have to agree with Neil, the figures quoted are well in excess of what we
find on a typical HASL board. With manufacturers trying to obtain the
flattest possible pads for fine pitch SM components, we've found it's not
uncommon to find Solderability issues arising from insufficient coverage,
particularly on the knee region of a PTH. Has anyone else seen this?
Ian Fox
Process Engineering Manager
TRW ASG
-----Original Message-----
From: Neil Atkinson [mailto:[log in to unmask]]
Sent: 22 October 2001 08:31
To: [log in to unmask]
Subject: Re: [TN] HASL Plating Thickness
I have been reading this thread with interest as I have a been asking this
question recently about some PCBs we have outsourced which are not as good
as our normal levelling.
Reading all of the e-mails and links I came to the conclusion that between
10 and 25 microns seems reasonable so the suggestion of 2.5 mils seems high
(if my conversions are right and 2.5mils is around 63.5 microns, back to the
old metric 'v' imperial argument!?!?!).
Does anyone out there quote a flatness spec for their HAL and if so, what do
you quote?
Neil
-----Original Message-----
From: Larry Tawyea [mailto:[log in to unmask]]
Sent: 19 October 2001 20:37
Subject: Re: HASL Plating Thickness
In a message dated 10/18/01 5:18:09 AM Central Daylight Time,
[log in to unmask] writes:
Christopher,
A thickness of 3.5 mils seems a little high but in my experience 2.5 mils
would not be out of the question.
Larry Tawyea
Hello All,
Is there any specification regarding the max thickness of HASL plated
PCB's. We have recently received a lot of boards where the HASL plating on
the fine pitch device exceeds 3.5 mils. He have an extensive amount of
bridging on these devices now. Any help would be greatly appreciated.
Thanks
Christopher Lampron
############################################################################
#########
Attention:
This message is for the named person's use only. It may contain
confidential,
proprietary or legally privileged information. No confidentiality or
privilege
is waived or lost by any mistransmission. If you receive this message in
error,
please immediately delete it and all copies of it from your system, destroy
any
hard copies of it securely and notify the sender. You must not, directly or
indirectly, use, disclose, distribute, print, or copy any part of this
message
if you are not the intended recipient. STADIUM GROUP PLC and any of its
subsidiaries
each reserve the right to monitor all e-mail communications through its
networks.
Any views expressed in this message are those of the individual sender,
except where
the message states otherwise and the sender is authorised to state them to
be the
views of Stadium Group Plc. or one of its subsidiaries.
Although this message has been scanned by MailMarshall for known viruses and
inappropriate content, we recommend that recipients employ appropriate
measures on
their systems to intercept any such material.
Thank You - Stadium Group Plc., IT Department - Tel: +44 (0)1429 266544
############################################################################
#########
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|