Sue,
If hole wall pullaway is not a defect, does it follow that it is an acceptable
condition? I ask only because we have thrown away many a pcb due to the hole
walls "exploding" or delaminating due to HASL stress, especially thick boards.
Also, if the hole wall pulls away, what about inner layer?
Just wondering, thought you'd be the expert to ask.
Joseph Spicuzza
Quality Assurance Supervisor
Advanced Interconnect Products Division
Compunetics, Inc.
ph: 412 858-6166
fax 412 373-8060
[log in to unmask]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To recieve ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|