Hi, Cathy,
No, the acceptable percentage of missed faults is zero, but with visual
inspection, it's accepted as a fact of life that only 80% of faults are
noticed at any time - partly because "pass" and "fail" conditions are
subjective up to a point, and partly because the human mind tends to
wander, and thoughts may be elsewhere at the time the eyes are passing over
a fault, so the fault doesn't register in the inspector's mind. It's
accepted, but not acceptable. The concern is the question of how serious
the faults are that aren't found. You can reasonably assume that major
defects will be spotted, but after 20+ years in this industry, I promise
you it's not just the minor faults that escape detection.
Unfortunately, we have no means of automating this sort of inspection work,
so we have to live with the imperfect yield of fault detection. We can
improve it a bit with training and awareness sessions for inspectors, but
even so, about 20% of faults are said not to be found. This does have an
effect of product life in the field, and field defects cost - money,
hassle, time, loss of customer confidence, resources to fix, etc.
I take it you have a yield problem? Or different inspectors find/miss
different faults?
Good luck with your bug hunt - I hope you find ways to reduce their
numbers.
Regards
Peter Duncan
Cathy Killen
<ckillen@SMTE To: [log in to unmask]
K.CO.UK> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST
Sent by: Aero/ST Group)
TechNet Subject: [TN] Solder Joint Defects
<[log in to unmask]
ORG>
10/18/01
07:33 PM
Please
respond to
"TechNet
E-Mail
Forum."
Could anyone help with this.
When visually inspecting PCBs to class 3, is there an acceptable percentage
of faults missed? Also is there an acceptable defect level considering PPM
with regards to soldered joints.
Cathy Killen
Training Instructor
Smtek Europe Ltd.
The information contained in the E-mail is confidential. It is intended
only
for the stated addressee(s) and access to it by any other person is
unauthorised.
The views expressed in this E-mail are those of the author, and do not
represent the views of Smtek Europe, its associates or subsidiaries, unless
otherwise expressly indicated.
Please note: It is your responsibility to scan this E-mail for viruses.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|