I've seen it done using crimp height as the variable and I've seen it done
using crimp pressure as the variable. If your machine monitors pressure it
works well. Crimp height is easier if you are checking samples.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]]On Behalf Of
> [log in to unmask]
> Sent: Wednesday, May 01, 2002 5:18 PM
> To: [log in to unmask]
> Subject: [TN] Crimp Tools
>
>
> I'm thinking about a different approach to monitor crimp tools
> using x-bar & r charts and was wondering if anyone out there is
> using similar methods.
> Your feedback is very much appreciated.
> Thanks,
> Rick Howieson
> Delta Group Electronics, Inc.
>
> ------------------------------------------------------------------
> ---------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ------------------------------------------------------------------
> ---------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|