I would not put anything other than 'silver saver' paper in direct contact
with silver plated product. That being said, On the opposite side of said
paper I add desiccant packs to ensure the proper environment (until the
customer opens the bags and stores the bare boards in an open bin in a non
controlled warehouse.
What your associate might have meant was not to have the pack in direct
contact with the silver finish...just my opinion.
Franklin
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Wednesday, March 05, 2008 10:53 AM
To: [log in to unmask]
Subject: [TN] Immersion Silver and Desiccants
One of my associates read somewhere (on a datasheet) that
desiccants should NOT be packaged with immersion silver boards,
(and seems to be putting a huge significance on that discovery)
My response would be:
OK. take out the desiccants and put in humidity indicators.
case closed.
Is there something else I should know about this?
Jack (aka "the new guy")
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|